廠家及牌號 | 試驗條件 | 測試方法 | 裝有測量儀表的落鏢沖擊 |
PPO(PPE)+PS 沙伯基礎 NORYL™ SE100HX resin (無溴,阻燃性,無氯,注射成型) | -30°C,EnergyatPeakLoad | ASTMD3763 | 3.28 J |
PPO(PPE)+PS 沙伯基礎 NORYL™ SE100X resin | -30°C,EnergyatPeakLoad | ASTMD3763 | 16.3 J |
PPO(PPE)+PS 沙伯基礎 NORYL GTX™ GTX626 resin (高耐熱性,耐化學性良好,擠出吹塑成型) | -30°C,EnergyatPeakLoad | ASTMD3763 | 36.6 J |
PPO(PPE)+PS 沙伯基礎 NORYL™ PPX640 resin (延高的拉伸率,高剛性注射成型填料:玻璃纖維增強材料, 40% 填料按重量。) | -30°C,TotalEnergy | ASTMD3763 | 14.1 J |
此文獻-版權所有-請勿轉載或其它用途.//shanglikaiguan.cn/ | |||
PPO(PPE)+PS 沙伯基礎 NORYL PPX™ PPX630 resin | -30°C,TotalEnergy | ASTMD3763 | 20.4 J |
PPO(PPE)+PS 沙伯基礎 NORYL PPX™ PPX630F resin (高剛性,延高的拉伸率,注射成型填料:玻璃纖維增強材料, 30% 填料按重量。) | -30°C,TotalEnergy | ASTMD3763 | 20.4 J |
PPO(PPE)+PS 沙伯基礎 NORYL GTX™ GTX902 resin (耐化學性良好,可噴涂的,注射成型) | -40°C,EnergyatPeakLoad | ASTMD3763 | 19.7 J |
PPO(PPE)+PS 沙伯基礎 NORYL PPX™ PPX640F resin (延高的拉伸率,高剛性注射成型填料:玻璃纖維增強材料, 40% 填料按重量。) | -30°C,TotalEnergy | ASTMD3763 | 14.1 J |
PPO(PPE)+PS 沙伯基礎 NORYL PPX™ PPX830 resin | -30°C,TotalEnergy | ASTMD3763 | 10.0 J |
PPO(PPE)+PS 沙伯基礎 NORYL GTX™ GTX910 resin (耐化學性良好,尺寸穩定性良好,注射成型) | -30°C,EnergyatPeakLoad | ASTMD3763 | 39.5 J |