廠家及牌號 | 試驗條件 | 測試方法 | CLTE-Transverse(-30to30°C) |
PA66 沙伯基礎 LNP™ STAT-KON™ RE0069S compound | ASTMD696 | 8.0E-6 cm/cm/°C | |
PA66 沙伯基礎 LNP™ THERMOCOMP™ RFB53XXZ compound | ASTMD696 | 8.4E-5 cm/cm/°C | |
PA66 沙伯基礎 LNP™ STAT-KON™ REL33 compound (潤滑,耐磨損性良好,導電,注射成型填料:碳纖維增強材料, 15% 填料按重量。) | ASTMD696 | 9.0E-6 cm/cm/°C | |
PA66 沙伯基礎 LNP™ LUBRICOMP™ RX06480 compound (阻燃性填料:玻璃纖維增強材料, 30% 填料按重量。) | ASTMD696 | 5.8E-5 cm/cm/°C | |
該文獻版權所有.請勿轉載或其它.用途.//shanglikaiguan.cn/ | |||
PA66 沙伯基礎 LNP™ LUBRICOMP™ RCL26 compound (導電,潤滑,耐磨損性良好,注射成型填料:碳纖維增強材料, 30% 填料按重量。) | ASTMD696 | 4.3E-5 cm/cm/°C | |
PA66 沙伯基礎 LNP™ LUBRICOMP™ RX85514 compound | ASTMD696 | 7.6E-5 cm/cm/°C | |
PA66 沙伯基礎 LNP™ THERMOCOMP™ RF007SXN compound (熱穩定性,水解穩定,注射成型填料:玻璃纖維增強材料, 35% 填料按重量。) | ASTMD696 | 6.3E-5 cm/cm/°C | |
PA66 沙伯基礎 LNP™ THERMOCOMP™ RF007H compound (注射成型填料:玻璃纖維增強材料, 35% 填料按重量。) | ASTMD696 | 7.3E-5 cm/cm/°C | |
PA66 沙伯基礎 LNP™ THERMOCOMP™ RF003AXH compound (注射成型填料:玻璃纖維增強材料, 15% 填料按重量。) | ASTMD696 | 7.8E-5 cm/cm/°C | |
PA66 沙伯基礎 LNP™ VERTON™ RV0079 compound | ASTMD696 | 4.8E-5 cm/cm/°C | |
溫馨提示 | |||
1.有關“CLTE-Transverse(-30to30°C) PA66”類數據資訊最多展示10條.更多牌號應用數據請向客服索取。 2.有關“PA66塑膠原料”類數據的實時性及更多塑膠原料行情敬請關注我們的資訊動態. |
● FEP 表面電阻率
● 其他熱塑性材料 彎曲強度5(斷裂,50.0mm跨距)
● TPE 空氣中拉伸強度的變化率(136°C,168hr)
● ABS+PET 懸壁梁缺口沖擊強度(3.20mm)
● PPA 拉伸應力(屈服,23°C)