廠家及牌號 | 試驗條件 | 測試方法 | 熔流率(熔體流動速率) |
PPO(PPE) 芬蘭普宓斯 PREPERM® 255 | 300°C/2.16kg | ISO1133 | 5.0 g/10min |
PPO(PPE) 沙伯基礎 NORYL™ WCP921A resin | 210°C/5.0kg | ASTMD1238 | 12 g/10min |
PPO(PPE) 沙伯基礎 NORYL™ WCP761 resin | 210°C/5.0kg | ASTMD1238 | 15 g/10min |
PPO(PPE) 沙伯基礎 LNP™ THERMOCOMP™ ZKC04 compound | 300°C/10.0kg | ASTMD1238 | 33 g/10min |
此文獻版權所有,請勿轉載或其它用途.//shanglikaiguan.cn/ | |||
PPO(PPE) 中國上海錦湖日麗 KumhoSunny PPO HSP8340 (良好的抗蠕變性,吸水低或不吸水,通用,注射成型) | 220°C/10.0kg | ASTMD1238 | 12到16 g/10min |
PPO(PPE) 沙伯基礎 NORYL™ NH4030B resin | 280°C/5.0kg | ASTMD1238 | 18 g/10min |
PPO(PPE) 韓國LG化學 Lumiloy® GN4356F (高強度,流動性高,注射成型填料:玻璃礦物, 35% 填料按重量。) | 280°C/5.0kg | ASTMD1238 | 19 g/10min |
PPO(PPE) 中國上海錦湖日麗 KumhoSunny PPO HSP8344 (抗撞擊性高,良好的抗蠕變性,吸水低或不吸水,注射成型) | 220°C/10.0kg | ASTMD1238 | 10到14 g/10min |
PPO(PPE) 沙伯基礎 NORYL™ WCP921 resin | 210°C/5.0kg | ASTMD1238 | 15 g/10min |
PPO(PPE) 沙伯基礎 NORYL GTX™ GTX951W resin (流動性高,注射成型) | 280°C/2.16kg | ASTMD1238 | 26 g/10min |